Dual Layer Crystal Sputter · 晶耀系列
Crafted with 4K Optical-Grade PET, Vireon Crystal™ features advanced Multi-Layer Magnetron Sputtering Technology, precisely depositing Tungsten Oxide (WO₃), Indium Tin Oxide (ITO), Nickel (Ni), Titanium (Ti), and Titanium Nitride (TiN) onto the film surface. At the core of its technology, Titanium Nitride (TiN) delivers exceptional infrared heat reflection for powerful heat dissipation and rapid cabin cooling. Combined with the broad-spectrum infrared rejection capabilities of WO₃ and ITO, Vireon Crystal™ provides outstanding heat insulation while maintaining 4K crystal-clear visibility, long-lasting color stability, and exceptional durability.


Swipe to compare all tiers →
| Specification | 74% VLT Vireon Crystal 7099 | 50% VLT Vireon Crystal 5099 | 35% VLT Vireon Crystal 3599 | 20% VLT Vireon Crystal 2099 | 5% VLT Vireon Crystal 0599 |
|---|---|---|---|---|---|
| UV Rejection (UVR) | 99% | 99% | 99% | 99% | 99% |
| IR Heat Rejection (IRR) | 99% | 99% | 99% | 99% | 99% |
| Solar Energy Rej. (TSER) | 58% | 65% | 77% | 83% | 91% |
| Thickness | 2mil | 2mil | 2mil | 2mil | 2mil |
| Scratch Resistance | 3H | 3H | 3H | 3H | 3H |
| Haze Value | 0.54% | 0.57% | 0.53% | 0.58% | 0.60% |
Swipe to compare all tiers →
Drag the slider to preview how each visible-light-transmittance level changes your view through the glass.

Infrared rays carry most of the sun's heat. The Vireon Crystal™ coating stack reflects them before they enter the cabin.
Drag the handle to compare glare and heat — bare glass vs Cool Cube film.